Textured Paint
SP ® THANE POLYURETHANE 2K COLOR COATING
MSP:
Product Description
- Characteristic
- Surface preparation
- Construction
- High adhesion, excellent ball durability.
- Hardened paint film, high wear and impact resistance.
- The surface to be painted must be clean, dry, free from grease, other impurities and not pollened. The compatible paint layer must be clean, dry and undamaged.
Please contact the manufacturer for advice.
- Stir the base part (part A) well with a hand tool or stirrer. Slowly pour the curing part (part B) into the container of part A in a ratio of 4 parts A and 1 part B. Stir thoroughly for about 3-5 minutes until the mixture is homogeneous.
- Use SP®TN304 diluent only when required (Maximum rate of 3% by mass of A & B mixture).
- The minimum construction surface temperature reaches 10 o C and 5 o C higher than the dew point of the air. The humidity of the construction environment ≤ 85%.
- Do not apply in the rain, early morning or late afternoon when there is dew to prevent the paint from fading
- Clean tools and equipment after construction with SPTHINNER 304.