SP ® DUR-EFN EPOXY COLOR PAINT - ROLLING/SPRAYING
MSP:
Product Description
- Characteristic
- Surface preparation
- Construction
- Good adhesion on metal, concrete.
- Excellent abrasion/ impact/ moisture/ chemical resistance, durable and anti-moss mold.
- Good heat resistance. The paint can be used for heated surfaces up to 1000C (discontinuous).
The painting surface must be clean, dry and free from oil, grease, other impurities and no chalking.
- Stir the base part (part A) with a stirrer. Slowly pour the curing portion (part B) into container has part A
at a rate of 4 parts A and 1 part B. Stir evenly for 3 minutes until the mixture is homogeneous.
- Use only solvent when required (maximum 3% by volume of A & B mix).
- Mixing should not be left exceed 5 hours at 230C.
- Cleaning tools and equipment after application with SPTHINNER 300 or SPTHINNER 305.
Color: | As shown on color board |
Solid content: | min 50% |
proportion: | 7 – 9 m2/kg/ 40 µm (depending on surface conditions) |
Theoretical coverage: | 1.2 ± 0.1 g/ml |
Mixing ratio A/B: | 4/1 (by volume) |
Film thickness: | Wet thickness: 80 - 100 µm Dry thickness: 40 -50 µm |
dried(23°C): | Touchable dry 4h Hard dry16h |
Time coating layer (23°C): | minimum after 6h |
Time live (after mixing): | 5 hours at 25oC |
Diluent: | SP®TN 300, 305 |
VOC: | Maximum 100g/kg |