Textured Paint
SP ® THANE POLYURETHANE 2K COLOR COATING
MSP:
Product Description
- Characteristic
- Surface preparation
- Construction
- Good adhesion, excellent gloss and durability.
- The paint film is hard, tough and has good abrison resistance.
- Good tolerance under extreme weather, UV and corrosive chemicals.
- Excellent tolerance under acid, alkaline, gasoline, water.
- Can be used for heated surfaces up to 1000C (discontinuous)
The painting surface must be clean, dry, non-chalky and free from oil or any contamination.
- Stir the base part (part A) with a stirrer. Slowly pour the curing portion (part B) into container A at a ratio of 4 parts A and 1 part B. Stir evenly for 3 minutes until the mixture is homogeneous.
- Use only thinner when required (maximum 3% by volume of A & B mix).
- Mixing should not be left exceed 5 hours at 23oC.
- Cleaning tools and equipment after application with SPTHINNER 304.
Color: | As request |
Solid content: | min 50% |
proportion: | 7 – 9 m2/kg/ 40 µm (Depending on surface) |
Theoretical coverage: | 1.3 ± 0.1 g/ml |
Mixing ratio A/B: | 4 / 1 (by volume) |
Film thickness: | Wet thickness: 80 µm Dry thickness: 40 µm |
dried(23°C): | touchable dry 4h hard dry 16h |
Time coating layer (23°C): | minimum after 16h |
Time live (after mixing): | 5 hours |
Diluent: | SPTHINNER 304 |